In accordance with the different processes of production, seamless steel
pipe is parallel to the longitudinal weld steel pipe
steel pipe, usually divided into metric welded steel pipe, welding thin-walled tube,
transformer cooling tubing. Seamless steel pipe has a different use of the value and role of
seamless steel pipe in use, in accordance with the appropriate method to use and welding
used in the welding process and precautions, welding procedure for seamless
pipes needs to be carried out in accordance with the production process.
The seamless high frequency welded steel pipe processing technology is relatively simple,
rapid, continuous production in the production process is simple and convenient, in
accordance with the process of production and processing. Seamless steel pipe is widely used
in civil construction, petrochemical, light industry and other sectors, low-pressure fluid
used for transport or made into a variety of engineering components and light industrial
products, play an important role in different industries and value, to show good
characteristics and performance.
Seamless steel pipe production process
Seamless steel pipe by high-frequency welding unit the strip strip certain specifications
volumes into round tubular and seamless welded steel pipe, welding processes and
technologies. Welding seamless steel pipe when the shape of the steel tube can be circular,
can also be a square or profiled, sizing rolling after the selection of the tube depends on
the welding of the welded steel pipe material, the material of the steel pipe, the main
production and processing technology will be different, the attention to the processing of
the material is low carbon steel and σs ≤ 300N/mm2 σs ≤ 500N/mm2 low alloy steel or other
steel. The welding technology is relatively simple, seamless steel pipe production and
processing technology to ensure that play an important role in the use and value, it
represents good value.
Seamless steel tubes for high-frequency welding technology
The high-frequency welding is a seamless steel pipe according to the principle of
electromagnetic induction, and AC charge in the skin effect of the conductor and the
proximity effect and eddy current heating effect, so that the weld edges of the steel
locally heated to a molten state, and the rollers squeeze the butt welding the purpose of
high-frequency welding seam crystal coupling, so as to achieve the weld is an induction
welding (contact or pressure welding), it does not require the weld filler, weld spatter,
narrow weld heat affected zone, welding forming beautiful subject to a wide range of
applications the welding good mechanical properties, etc., in the production of steel pipe
seamless steel pipe of high-frequency welding is the use of alternating current skin effect
and proximity effect, steel (steel) after roll forming to form a section off a circular
tube, in the tube near the induction coils near the center of rotation or a group the
impedance (Cibang), an electromagnetic induction circuit is formed by the impedance with the
blank tube openings in the skin effect and proximity effect, under the action of the edge of
the blank tube openings generating a strong and concentrated thermal effect, so that the
weld edges welding rapidly heated to the desired temperature after extrusion by the pressure
roller, the molten state of the metal crystal indirectly together, cooling to form a solid
after docking weld.
Seamless steel pipe welding technology needs to grasp and control during welding, to ensure
that the welding steel pipe without quality and performance issues and quality, play an
important role and value in use.